Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 28 mm/min @Thickness 1.00 mm |
1.1 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® S600F40 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 BK851 is an unreinforced lubricated low viscosity black polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Flame Spread | 28 mm/min @Thickness 1.00 mm |
1.1 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |