EG85A-B40 Polyurethane-based Biomedical Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EG85A-B40 Polyurethane-based Biomedical Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
ASTM D2240
Tensile Strength, Ultimate 35.11 MPa
5093 psi
ASTM D412
Elongation at Break 559 %
559 %
ASTM D412