Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 32.9 g/10 min @Load 2.16 kg, Temperature 250 °C |
32.9 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 32.9 g/10 min @Load 2.16 kg, Temperature 250 °C |
32.9 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® S600F40 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 BK851 is an unreinforced lubricated low viscosity black polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Melt Flow | 32.9 g/10 min @Load 2.16 kg, Temperature 250 °C |
32.9 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |