Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating  (discontinued **)<

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Coating Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating  (discontinued **)<.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resins.Features/Benefits vs. Nucrel® 0910HS: Slip additives are added to reduce the coefficient of friction of the film surface to increase operating speeds on packaging machinery. Chill roll release agents are added to enhance extrusion coating speeds by reducing tendency of the hot melt to adhere to the chill roll surface Typical Applications: Medical/pharmaceutical packaging; Condiment and miscellaneous nonfood pouches; Snack structures; Heat seal applications using vertical form-fill-seal packaging machinery.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength 1500 g/25 mm
1500 g/in
seal bar 140°C.
Hot Tack Strength 1000 g/25 mm
1000 g/in
seal bar 110°C; DuPont Spring Test Method
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
103 °C
217 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 290 °C
554 °F
Typical Die Temp.
Melt Temperature 260 - 305 °C
500 - 581 °F