Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 183 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Internal Method
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f..
Melting Point 84.0 °C
183 °F
DSC
Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)
7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr..
Melting Point 84.0 °C
183 °F
Exxon Method
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
9.2 wt% Methacrylic Acid.Nucrel® 0908HS is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and blown/cast film operations desi..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 0910HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
8.7 wt% Methacrylic Acid.Nucrel® 0910HS (High-Stability) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating and extrusion lamin..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 407 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
4 wt% Methacrylic Acid.Nucrel® 0407 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment desi..
Melting Point 84.0 °C
183 °F
ASTM D3418, ISO 3146
DuPont™ Elvax® 440 Ethylene Vinyl Acetate
DuPont™ Elvax® 440 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. ELVAX® 440 EVA Resin complies with Food and Drug Administration Regulation 21 CFR 177.1350(a)(1..
Melting Point 84.0 °C
183 °F
DSC
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium
Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and ..
Melting Point 84.0 °C
183 °F
DSC
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam..
Melting Point 84.0 °C
183 °F
10°C/min
Arkema Group Evatane® 1350 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets.ISO data provided by the manufacturer, Arkema.
Melting Point 84.0 °C
183 °F
ASTM D3417
DuPont Elvax® 3176CW-3 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 3176CW-3 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additi..
Melting Point 84.0 °C
183 °F
Exxon Method
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature ..
Melting Point 84.0 °C
183 °F
Freezing Point via DSC/ASTM D3418
DuPont Nucrel® 0910HS-SR Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating  (discontinued **)<
8.7 wt% Methacrylic Acid.Nucrel® 0910HS-SR is an ethylene-methacrylic acid copolymer resin available for use in conventional and coextrusion coating equipment designed to process polyethylene resin..
Melting Point 84.0 °C
183 °F
Exxon Method
ExxonMobil Escorene® LD-724 High EVA Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty compounding applications. Outstanding heat sealability along with excellent strength properties ..
Copyright © lookpolymers.com All Rights Reserved