Material Notes:
DuPont™ Elvax® 440 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. ELVAX® 440 EVA Resin complies with Food and Drug Administration Regulation 21 CFR 177.1350(a)(1) - - Ethylene-vinyl acetate copolymers, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (b)(1) of the Regulation.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D792, ISO 1183
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
ASTM D3418, ISO 3146
Vicat Softening Point 53.0 °C
127 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F