Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 53.0 °C | 127 °F | Vicat A, 1 kg; DIN 53460/ISO 306 |
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | ASTM D1525 |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Vicat Softening Point | 53.0 - 160 °C | 127 - 320 °F | Average value: 113 °C Grade Count:112 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | ASTM D1525 |
Westlake EMAC® SP2202 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2202 is a 21.5% EMA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2202 provides exce.. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | ASTM D1525 |
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | |
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 53.0 °C | 127 °F | ASTM D1525, ISO 306 |
DuPont™ Elvax® 440 Ethylene Vinyl Acetate DuPont™ Elvax® 440 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. ELVAX® 440 EVA Resin complies with Food and Drug Administration Regulation 21 CFR 177.1350(a)(1.. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and .. |
|||
Vicat Softening Point | 52.8 °C | 127 °F | Peak Melting Temperature; ASTM D1525 |
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f.. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | ASTM D1525 |
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a.. |
|||
Vicat Softening Point | 53.0 °C @Load 1.02 kg |
127 °F @Load 2.25 lb |
ASTM D1525 |
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of .. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | |
Biomer P240 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | 50°C/hr; 50N |
Arkema Group Evatane® 1350 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 53.0 °C | 127 °F | |
BASF Novolen® 3300 MC Polypropylene Data was collected by ISO methods and provided by BASF. |