Pyrotek TS-105 Thermoset Electrical Insulation Product (Nema Grade: G-5)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Melamine
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek TS-105 Thermoset Electrical Insulation Product (Nema Grade: G-5).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass reinforcement, Melamine Resin, Gray color. High mechanical strength, arc and heat resistance. Self-extinguishing.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasketsAdvantagesHigh insulation properties High strength Low moisture absorption High temperature resistance Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
Water Absorption 0.40 %
0.40 %
Mechanical Properties Metric English Comments
Flexural Strength 345 MPa
50000 psi
Compressive Strength 448 MPa
65000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm
Dielectric Strength 12.0 kV/mm
305 kV/in
Arc Resistance 180 sec
180 sec