Spartech Soft Touch R-104 Laminated Sheet Specialty Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name Soft Touch
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Soft Touch R-104 Laminated Sheet Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.03 - 1.05 g/cc
1.03 - 1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 190 %
190 %
ASTM D638
Flexural Yield Strength 57.2 MPa
8300 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Unnotched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648
Descriptive Properties Value Comments
Flammability Passes
MVSS (Motor Vehicle Safety Standard) 302