DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent drawability for easy processing, good flex-crack resistance for liquid packaging, high toughness, low shrink for water bath applications, and excellent optical properties. It adheres to many materials. It is commonly used as a tie layer in certain coextrusions with dissimilar surfaces.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Moisture Vapor Transmission 1.34 cc-mm/m²-24hr-atm
3.40 cc-mil/100 in²-24hr-atm
g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
Oxygen Transmission 197 cc-mm/m²-24hr-atm
500 cc-mil/100 in²-24hr-atm
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
Melt Flow 1.5 g/10 min
1.5 g/10 min
Condition not noted.; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 580 %
580 %
MD-TD Average; ASTM D882
Film Elongation at Break, TD 580 %
580 %
MD-TD Average; ASTM D882
Impact 29.4
29.4
J/mm Spencer Impact; ASTM D3420; Average of MD and TD
Elmendorf Tear Strength, MD 3.82 g/micron
97.0 g/mil
Average of MD and TD; ASTM D1922
Film Tensile Strength at Break, MD 29.0 MPa
4210 psi
MD-TD Average; ASTM D882
Thermal Properties Metric English Comments
Melting Point 68.0 °C
154 °F
Freezing Point via DSC/ASTM D3418
89.0 °C
192 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 68.0 °C
154 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 48 %
48 %
ASTM D1003
Gloss 22 %
22 %
20°; ASTM D2457