Polymer Property : Oxygen Transmission = 500 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 197 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
500 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Oxygen Transmission 197 - 200 cc-mm/m²-24hr-atm
500 - 508 cc-mil/100 in²-24hr-atm
Average value: 199 cc-mm/m²-24hr-atm Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Oxygen Transmission 197 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
500 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
8.9 wt% Vinyl Acetate.Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resin..
Oxygen Transmission 197 cc-mm/m²-24hr-atm
500 cc-mil/100 in²-24hr-atm
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film  (discontinued **)
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..