Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 3.82 g/micron | 97.0 g/mil | Average of MD and TD; ASTM D1922 |
DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **) 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |