Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-gap equipment. It contains high level of slip additive and medium level of antiblock additive. This material complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.1 (a) for food packaging applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
Melt Flow 0.85 g/10 min

@Load 2.16 kg
0.85 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
Coefficient of Friction 0.17
0.17
Film Tensile Strength at Break, MD 32.0 MPa
4640 psi
Film Tensile Strength at Break, TD 32.0 MPa
4640 psi
Thermal Properties Metric English Comments
Vicat Softening Point 103 °C
217 °F
Optical Properties Metric English Comments
Haze 12 %
12 %
Gloss 54 %
54 %
45°
Processing Properties Metric English Comments
Processing Temperature 226 °C
439 °F
Film extrusion temperature