Dow Corning JCR 6109

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning JCR 6109.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, translucent, low modulus LED gel encapsulant with a very long working time.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc

@Temperature 25.0 °C
1.04 g/cc

@Temperature 77.0 °F
Viscosity 3900 cP
3900 cP
dynamic
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 167
167
Optical Properties Metric English Comments
Refractive Index 1.414
1.414
1.424
1.424
1.413

@Wavelength 1554 nm
1.413

@Wavelength 1554 nm
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+15 ohm-cm
1.80e+15 ohm-cm
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
Dielectric Strength 18.00 kV/mm
457.2 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 70.0 °C
1.00 hour

@Temperature 158 °F
960 min

@Temperature 150 °C
16.0 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance translucent