Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3900 cP | 3900 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1101 K (SBS) Liner Block Copolymer Kraton D1101 K is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified:Kraton D1101 .. |
|||
Viscosity | 3900 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3900 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C10903P14 Carbon/Graphite Ink Carbon Graphite Ink is used for screen printing working electrodes. This is a carbon graphite ink, which has been optimized to give superior electrochemical performance with good reversibility when.. |
|||
Viscosity | 3900 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3900 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake Viscosity |
Gwent Electronic Materials C60531D1 Silver / Silver Chloride Paste C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa.. |
|||
Viscosity | 3900 cP @Temperature 25.0 °C |
3900 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Viscosity | 3900 cP | 3900 cP | dynamic |
Dow Corning JCR 6109 One-part, translucent, low modulus LED gel encapsulant with a very long working time.Information provided by Dow Corning |
|||
Viscosity | 3900 cP @Temperature 204 °C |
3900 cP @Temperature 400 °F |
Typical |
Bostik 6239 Low Viscosity, High Temp Resistance, Long Open Time Polyamide Glue Stick Bostik 6239 Low Viscosity, High Temp Resistance, Long Open Time Polyamide Glue StickLow application viscosity. High temperature resistance. Long open time. Resistance to plasticizer migration for vi.. |