Polymer Property : Dielectric Strength = 18.00 kV/mm
Polymer Property :
Dielectric Strength =
18.00 kV/mm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Dielectric Strength
18.00
kV/mm
457.2
kV/in
Dow Corning JCR 6109
One-part, translucent, low modulus LED gel encapsulant with a very long working time.Information provided by Dow Corning