Dow C719-35RNHP Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C719-35RNHP Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewHigh impactContains a nucleating agentControlled rheology productComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C719-35RNHP Polypropylene Resin is intended for use in injection molding applications requiring a good impact/stiffness balance.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
DSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Unannealed; ASTM D648