Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow C700-35N Polypropylene Impact Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow C700-35N Polypropylene Impact Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OverviewGood mold fillabilityHigh stiffnessFast set-upContains a nucleating additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35N Polypropylene Resin is intended for use in injection molding processes where medium impact strength is required. This product contains a nucleating additive.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus, 1% Secant 1520 MPa
220000 psi
ASTM D790A
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: