Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1520 MPa | 220000 psi | ASTM D790A |
SABIC PP 511A Polypropylene Homopolymer for Spunbond Applications Product Description: PP 511A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 511A has the following features:Consis.. |
|||
Flexural Modulus, 1% Secant | 1517 MPa | 220000 psi | ASTM D790 |
Flint Hills AP5106-HA Polypropylene Impact Copolymer Features: Excellent impact stiffness balance, good mold release.Applications: Compression and injection molding: caps and closuresInformation Provided by Flint Hills Resources |
|||
Flexural Modulus, 1% Secant | 1517 MPa | 220000 psi | ASTM D790 |
Flint Hills AP5206-HN Polypropylene Impact Copolymer Features: Nucleated for fast cycle and good mold release. Product does not contain animal derived components.Applications: Compression and injection molding: caps and closuresInformation Provided b.. |
|||
Flexural Modulus, 1% Secant | 1520 MPa | 220000 psi | ASTM D790 |
Flint Hills P4G3Z-050F Polypropylene Homopolymer Features: Low Water Carry-over, good film quality. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: cast filmInformation Provided by Flint Hills Resource.. |
|||
Flexural Modulus, 1% Secant | 1520 MPa | 220000 psi | ASTM D790A |
Dow C700-35N Polypropylene Impact Copolymer Resin OverviewGood mold fillabilityHigh stiffnessFast set-upContains a nucleating additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35N Polypropylene Resin is intended for use in.. |
|||
Flexural Modulus, 1% Secant | 1520 MPa | 220000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |