Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Viscosity Measurement 0.800
0.800
Intrinsic Viscosity; ASTM D4603
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.7 MPa
10400 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 3.9 %
3.9 %
ASTM D638
Elongation at Yield 2.9 %
2.9 %
ASTM D638
Flexural Strength 94.4 MPa
13700 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.577 GPa
373.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 0.267 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.500 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Gardner Impact >= 0.960 J

@Temperature 23.0 °C
>= 0.708 ft-lb

@Temperature 73.4 °F
ASTM D5420
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified