Polymer Property : Flexural Modulus = 373.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.577 GPa
373.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.577 GPa
373.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP 60-3302 Clear Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.577 GPa
373.8 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP 60-8419G Clear Amorphous Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.