Gardner Impact >= 0.960 J

@Temperature 23.0 °C
>= 0.708 ft-lb

@Temperature 73.4 °F
ASTM D5420
Diamond Polymers NPP 60-8419G Clear Amorphous Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.