Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.365 g/cc
0.04931 lb/in³
JIS-Z-8807
Deformation 10 %
10 %
JIS-K-6723
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
JIS-K-6301
Tensile Strength at Break 15.696 MPa
2276.5 psi
JIS-K-6723
Elongation at Break 330 %
330 %
JIS-K-6723
100% Modulus 0.0090252 GPa
1.3090 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -32.0 °C
-25.6 °F
JIS-K-6723
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm

@Temperature 30.0 °C
1.00e+13 ohm-cm

@Temperature 86.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 82
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 96
JIS-A-5756
Oil Resistance: Retention of Tensile Strength, % 96
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 82
JIS-K-6723
Thermostability, min, JIS-K-6723 >240