Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0090252 GPa | 1.3090 ksi | JIS-A-5756 |
Denka VINYKON M7100 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0090252 GPa | 1.3090 ksi | JIS-A-5756 |
Denka VINYKON W2085 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0090252 GPa | 1.3090 ksi | JIS-A-5756 |
Denka VINYKON M556070 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |