Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ceradyne CeraTrex™ SC-P3 Silicon Carbide

Category Ceramic , Carbide
Manufacturer Ceradyne Advanced Ceramics
Trade Name CeraTrex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne CeraTrex™ SC-P3 Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 2850
2850
0.3
Modulus of Elasticity 440 GPa
63800 ksi
Flexural Strength 375 MPa

@Temperature 23.0 °C
54400 psi

@Temperature 73.4 °F
Poissons Ratio 0.17
0.17
Fracture Toughness 3.10 MPa-m½
2.82 ksi-in½
Shear Modulus 188 GPa
27300 ksi
calculated
Abrasion 1178
1178
Abrasive Wear Resistance Parameter
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 1000 °C
2.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 200 W/m-K
1390 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 3000 ohm-cm
3000 ohm-cm
Descriptive Properties Value Comments
Purity, % 99.9995
Thermal Shock Parameter 157°C
Users viewing this material also viewed the following: