DSM Fibre Intermediates Nyrim® 4000 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer DSM Fibre Intermediates
Trade Name Nyrim®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Fibre Intermediates Nyrim® 4000 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength, Ultimate 26.0 MPa
3770 psi
ISO 527
Elongation at Break 420 %
420 %
ISO 527
Modulus of Elasticity 0.453 GPa
65.7 ksi
ISO 527
Flexural Modulus 0.504 GPa
73.1 ksi
ISO 178
Shear Modulus 0.200 GPa
29.0 ksi
torsional
Thermal Properties Metric English Comments
Melting Point 214 °C
417 °F
DSC