Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cyclewood Solutions Xylomer™ XM2-JNA Sustainable Injection Molding Resin

Category Polymer , Renewable/Recycled Polymer , Thermoplastic
Manufacturer Cyclewood Solutions
Trade Name Xylomer™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cyclewood Solutions Xylomer™ XM2-JNA Sustainable Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100% biodegradable and compostable thermoplastic. The sustainable bio-based resin properties perform between polypropylene and polystyrene. Xylomer™ is modified lignin, an abundant, natural byproduct of the paper manufacturing process, blended with other compostable polymers. Xylomer™ pellets have been demonstrated in injection molding and vacuum forming processes to create samples of cups and bowls.Information provided by Cyclewood Solutions.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Melt Flow 33.9 g/10 min

@Temperature 230 °C
33.9 g/10 min

@Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength 29.04 MPa
4212 psi
Elongation at Break 1.8 %
1.8 %
Flexural Modulus 2.00 GPa
290 ksi
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in