Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Property data for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Flexural Yield Strength 190 MPa
27600 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.840 J/cm
1.57 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
306 °F
ASTM D648