Polymer Property : Tensile Strength, Yield = 17300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Tensile Strength, Yield 119 MPa

@Temperature 100 °C
17300 psi

@Temperature 212 °F
ISO 527
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Tensile Strength, Yield 119 MPa
17300 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI
LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding.
Tensile Strength, Yield 119 MPa
17300 psi
ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific)
LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2110EPR PEI
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Tensile Strength, Yield 119 MPa
17300 psi
ISO 527
SABIC Innovative Plastics LNP STAT-KON DE0039 PC
LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive.
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Techmer ES HiFill® PA6 GF/M40 HS L BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackProc..
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Techmer ES HiFill® PA6 GF/M40 IG BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedProcessing Method: In..
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
Tensile Strength, Yield 119 MPa
17300 psi
ISO 527
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific)
LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant.
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Tensile Strength, Yield 119 MPa
17300 psi
SABIC - Japan Method
SABIC Innovative Plastics NORYL CN5258 PPE+PS (Asia Pacific)
40% filled FR high modulus PPE/PS blend
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK)
TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels..
Tensile Strength, Yield 119 MPa

@Temperature -40.0 °C
17300 psi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8270 HS PA6 (Conditioned)
Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi..
Tensile Strength, Yield 119 MPa

@Temperature -40.0 °C
17300 psi

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8270 HS PA6 (Conditioned)
Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi..
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Tensile Strength, Yield 119 MPa
17300 psi
ASTM D638
Custom Resins Vexel™ 4200 RD PBT; 30% Glass Filler  (discontinued **)
Property data for dry as molded samples.Data provided by the manufacturer
Tensile Strength, Yield 119 MPa
17300 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10
LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant.