Material Notes:
Neat resin, for compounding.Information provided by Cresset Powers Ltd.
Physical Properties Metric English Comments
Density 1.12 - 1.14 g/cc
0.0405 - 0.0412 lb/in³
ASTM D792
Apparent Bulk Density >= 0.659 g/cc
>= 0.0238 lb/in³
Viscosity Measurement 2.7
2.7
Relative Viscosity
Melt Flow 14 - 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 - 20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 220 - 224 °C
428 - 435 °F
ASTM DSC
Deflection Temperature at 1.8 MPa (264 psi) >= 55.0 °C
>= 131 °F
Processing Properties Metric English Comments
Moisture Content <= 0.080 %
<= 0.080 %
Descriptive Properties Value Comments
Extractables, wt% <0.4