Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | >= 0.659 g/cc | >= 0.0238 lb/in³ | |
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, 50% RH Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | >= 0.659 g/cc | >= 0.0238 lb/in³ | |
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | >= 0.659 g/cc | >= 0.0238 lb/in³ | |
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, 50% RH Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Apparent Bulk Density | >= 0.659 g/cc | >= 0.0238 lb/in³ | |
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |