Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTAPROP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ASTM D 955
Melt Flow 1.0 - 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 - 4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D 638
Elongation at Break 1.6 %
1.6 %
ASTM D 638
Tensile Modulus 5.20 GPa
754 ksi
ASTM D 638
Flexural Modulus 4.30 GPa
624 ksi
ASTM D 790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 112 °C

@Load 5.10 kg
234 °F

@Load 11.2 lb
50°C/hr; ASTM D 1525
Electrical Properties Metric English Comments
Surface Resistance <= 3000 ohm
<= 3000 ohm
ASTM D257
Users viewing this material also viewed the following: