Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.20 GPa | 754 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 GF 15 002/1M PA66 reinforced with glass fiber PA66 for injection molding, reinforced with 15 % glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools,.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ASTM D638 |
NCMT NanoPAC™ G1550S High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Tensile Modulus | 5.20 - 18.2 GPa | 754 - 2640 ksi | MD |
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co.. |
|||
Tensile Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, glass fiber, injection molding, impact modified, heat-aged stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | |
LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled Dissipative product based on Polypropylene homopolymer (PPh). Mica filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Tensile Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ASTM-D790 |
Polyram RamOfin PPC364I6 Polypropylene, 30% Mineral and Glass Fiber 30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-25 HM PA6-GF25 Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AK8 PA66, 40% Mineral Reinforced, Injection Molding Staramide AK8 is a 40% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry) Ultramid 8262G HS BK-102 is a heat stabilized, pigmented black, 20% glass and mineral reinforced PA6 injection molding compound resulting in a balance of engineering properties with excellent dimens.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | ISO 527 |
BASF Ultramid® A3W2G6 BK 20560 30% Glass Filled PA66 (Conditioned) Description: Ultramid A3W2G6 BK20560 is a developmental 30% glass fiber reinforced, pigmented black, injection molding PA66/6 with high heat aging resistance.Applications: Automotive power train app.. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.20 GPa | 754 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |