CoorsTek ACI-Ni10 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek ACI-Ni10 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Physical Properties Metric English Comments
Density 14.4 g/cc
0.520 lb/in³
Particle Size 3.0 - 5.0 µm
3.0 - 5.0 µm
Grain Size
Mechanical Properties Metric English Comments
Hardness, Rockwell A 90
90
Modulus of Elasticity 572 GPa
83000 ksi
Flexural Strength 2930 MPa
425000 psi
Poissons Ratio 0.23
0.23
Shear Modulus 233 GPa
33800 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 25.0 - 400 °C
3.00 µin/in-°F

@Temperature 77.0 - 752 °F
5.60 µm/m-°C

@Temperature 25.0 - 800 °C
3.11 µin/in-°F

@Temperature 77.0 - 1470 °F
Specific Heat Capacity 0.215 J/g-°C
0.0514 BTU/lb-°F
Thermal Conductivity 75.0 W/m-K
521 BTU-in/hr-ft²-°F