Polymer Property : Shear Modulus = 33800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 233 GPa
33800 ksi
Calculated
CoorsTek ACI-Ni10 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries