Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Covestro
Trade Name Bayfill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.0960 g/cc
0.00347 lb/in³
Molded density, ASTM D3574-A
Apparent Bulk Density 0.0400 g/cc
0.00145 lb/in³
Free-rise Density, Bayer test
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.290 MPa
42.1 psi
ASTM D3574E
Elongation at Break 50 %
50 %
ASTM D3574E
Compressive Yield Strength 0.0620 MPa
8.99 psi
40% Compression, ASTM D3574-C
Tear Strength 1.20 kN/m
6.85 pli
Die C; ASTM D624
Compression Set 39 %
39 %
Test D, ASTM D3574 Dry