Density >= 14.4 g/cc
>= 0.520 lb/in³
Hogen H35S, 35 Silver/65 Tungsten PM Metal Composite
Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Silver-Tungsten is used when high oxidation-resistant materials are necessar..
Density >= 14.4 g/cc
>= 0.520 lb/in³
Mi-Tech Metals SW65 35 Silver/65 Tungsten PM Metal Composite
Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Silver-Tungsten is used when high oxidation-resistant materials are necessary and s..
Density 14.4 g/cc
0.520 lb/in³
Goodfellow Copelmet® Tungsten 72/Copper 28 Alloy
Developed as an electrode material, this alloy is used for spark erosion electrodes and contacts giving excellent resistance to mechanical wear and electrical erosion.Information provided by Goodfel..
Density 14.4 g/cc
0.520 lb/in³
CoorsTek ACI-Ni10 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Density 14.4 - 14.7 g/cc
0.520 - 0.531 lb/in³
China Tungsten K05 Tungsten Carbide for Mining Purposes
High toughness, wear resistance and performance, for single line and cross bits of rotary hammer rock drills for hard rock formations.Information provided by China Tungsten
Density 14.4 - 14.6 g/cc
0.520 - 0.527 lb/in³
China Tungsten K520 Tungsten Carbide for Mining Purposes
High toughness, wear resistance and complex properties, for bits of hammer rock drills and heavy rock drills for cutting hard rocks.Information provided by China Tungsten
Density 14.4 g/cc
0.520 lb/in³
China Tungsten YG11 Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.4 g/cc
0.520 lb/in³
China Tungsten YG11X Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.4 g/cc
0.520 lb/in³
China Tungsten YG813 Tungsten Carbide
Optimum wear resistance, high bending strength and high resistance to bonding . Machining of refractory alloys, stainless steel and high manganese steel, etc.Information provided by China Tungsten
Density 14.4 g/cc
0.520 lb/in³
China Tungsten YG11C Tungsten Carbide Powder
Information provided by China Tungsten
Density 14.4 - 14.6 g/cc
0.520 - 0.527 lb/in³
China Tungsten Z30 Tungsten Carbide for Mining Purposes
High toughness and wear resistance and good versatility, for rotary hammer rock drill bits and heavy rock drill bits, for f16~f18 hard and medium hard rocks formationsInformation provided by China T..