ChevronTexaco Multigear® EP SAE 85W-140

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Multigear® EP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Multigear® EP SAE 85W-140.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties protect hypoid and other types of gears from scuffing and wear under heavily loaded conditions.Long lubricant life — Outstanding thermal and oxidation stability allow high temperature operation with long lubricant life without the formation of sludge and deposits.All-weather protection — Multiviscosity characteristics assure proper gear lubrication at both low and high ambient temperatures.Corrosion and rust protection — Effective inhibitor package prevents rusting or corrosion of gears and bearings surfaces.Texaco Multigear EP oils are multipurpose lubricants.They are made with:Highly refined base stocksA carefully balanced additive package to provide maximum gear protection, long lubricant life and excellent field performanceSulfur-phosphorus extreme pressure additives that provide superior thermal and oxidation stabilityRust and corrosion inhibitors, a foam inhibitor, and a pour point depressantThe highly refined base stocks and various inhibitors in the additive package assure a well-balanced lubricant and long gear and bearing life with maximum durability.Texaco Multigear EP oils are recommended for use in all spiral bevel and hypoid differentials, power dividers, and oil-lubricated steering axle wheel bearings.They are designed for complete refill and make-up of all passenger car, light duty and heavy duty truck transmissions, conventional differentials and steering gears.Their multiviscosity characteristics allow their use in equipment operating over a broad ambient temperature range. This means good cold flow properties and gear protection.Texaco Multigear EP oils meet the performance requirements of:API Service Categories MT-1, GL-4, and GL-5Are qualified for SAE J 2360 (formerly known as MIL-PRF-2105E)They also meet the requirements of:A Mack GO-J fluidRockwell 0-76D (SAE 80W-90), 0-76-A (SAE 85W-140)Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222317; MSDS Number: 8628
Physical Properties Metric English Comments
API Gravity 25.9 °
25.9 °
Brookfield Viscosity 102000 cP

@Temperature -12.0 °C
102000 cP

@Temperature 10.4 °F
Viscosity Measurement 95
95
Viscosity Index
Saybolt Viscosity at 100°F 1819 SUS
1819 SUS
Saybolt Viscosity at 210°F 124 SUS
124 SUS
Kinematic Viscosity at 40°C (104°F) 341 cSt
341 cSt
Kinematic Viscosity at 100°C (212°F) 25 cSt
25 cSt
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 229 °C
444 °F