Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco Delo® SAE 85W-140 Gear Lubricant ESI® FeaturesChevron Delo Gear Lubricants ESI are premium grade, multipurpose gear lubricants.They are formulated with ISOSYN® base stocks and compounded with a unique extreme pressure additive utilizin.. |
|||
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco Havoline® SAE 85W-140 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco Multigear® EP SAE 85W-140 Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties.. |
|||
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco RPM® SAE 85W-140 Universal Gear Lubricant FeaturesChevron RPM Universal Gear Lubricants are multipurpose lubricants.They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protecti.. |
|||
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco TEGRA® SAE 80W-140 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality, multipurpose gear lubricants.It is manufactured from synthesized hydrocarbon base fluids which have exceptional thermal and oxid.. |
|||
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco Drive Train Fluid HD, SAE 60 FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Saybolt Viscosity at 210°F | 124 SUS | 124 SUS | |
ChevronTexaco Ulti-Plex® NLGI 2 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |