Polymer Property : Saybolt Viscosity at 100°F = 1819 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1819 SUS
1819 SUS
ChevronTexaco Delo® SAE 85W-140 Gear Lubricant ESI®
FeaturesChevron Delo Gear Lubricants ESI are premium grade, multipurpose gear lubricants.They are formulated with ISOSYN® base stocks and compounded with a unique extreme pressure additive utilizin..
Saybolt Viscosity at 100°F 1819 SUS
1819 SUS
ChevronTexaco Havoline® SAE 85W-140 Gear Oil
Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life..
Saybolt Viscosity at 100°F 1819 SUS
1819 SUS
ChevronTexaco Multigear® EP SAE 85W-140
Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties..