Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 229 °C | 444 °F | |
ChevronTexaco Havoline® SAE 85W-140 Gear Oil Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life.. |
|||
Flash Point | 229 °C | 444 °F | |
ChevronTexaco Multigear® EP SAE 85W-140 Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties.. |
|||
Flash Point | 229 °C | 444 °F | ASTM D92 |
ChevronTexaco RPM® SAE 85W-140 Universal Gear Lubricant FeaturesChevron RPM Universal Gear Lubricants are multipurpose lubricants.They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protecti.. |
|||
Flash Point | 229 °C | 444 °F | ASTM D92 |
ChevronTexaco Superla® 35 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Flash Point | 229 °C | 444 °F | |
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |
|||
Flash Point | 229 °C | 444 °F | |
ConocoPhillips El Mar® 3000 Oil SAE Grade 15W-40 Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such.. |
|||
Flash Point | 229 °C | 444 °F | |
ConocoPhillips Hydroclear® El Mar® 15W-40 Ashless Heavy Duty Description: Conoco Hydroclear El Mar Ashless Heavy Duty is a high-quality, ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Heavy D.. |
|||
Flash Point | 229 °C | 444 °F | ASTM D92 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Flash Point | 229 °C | 444 °F | ASTM D92 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |