Polymer Property : Saybolt Viscosity at 210°F = 124 SUS Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco Delo® SAE 85W-140 Gear Lubricant ESI®
FeaturesChevron Delo Gear Lubricants ESI are premium grade, multipurpose gear lubricants.They are formulated with ISOSYN® base stocks and compounded with a unique extreme pressure additive utilizin..
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco Havoline® SAE 85W-140 Gear Oil
Havoline Gear Oils are multipurpose lubricants. They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protection and long lubricant life..
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco Multigear® EP SAE 85W-140
Texaco Multigear EP oils deliver value through:Improved durability — Specially formulated to stand up to the demands of severe service applications.Extended gear life — Extreme pressure properties..
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco RPM® SAE 85W-140 Universal Gear Lubricant
FeaturesChevron RPM Universal Gear Lubricants are multipurpose lubricants.They are made from paraffinic base stocks and contain a carefully balanced additive package to provide maximum gear protecti..
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco TEGRA® SAE 80W-140 Synthetic Gear Lubricant
FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality, multipurpose gear lubricants.It is manufactured from synthesized hydrocarbon base fluids which have exceptional thermal and oxid..
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco Drive Train Fluid HD, SAE 60
FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 ..
Saybolt Viscosity at 210°F 124 SUS
124 SUS
ChevronTexaco Ulti-Plex® NLGI 2 Greases EP
FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The..