Material Notes:
Texaco Marfak Multipurpose delivers value through:Good water resistance — Provides lubrication in the presence of water.Good corrosion protection — Inhibited to protect gear and bearing surfaces.Good oxidation stability — Helps to ensure long life in storage and in use.Simplified lubrication — One grease designed to satisfy most general purpose, non-EP grease requirements.Texaco Marfak Multipurpose is manufactured using selected, highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thickener, and rust and oxidation inhibitors.It is work stable and resists separation or throw out from antifriction bearings. It has a low oil bleeding tendency under pressure and is pumpable at low temperatures.Texaco Marfak Multipurpose satisfies general automotive and industrial applications that do not require the use of an EP grease.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 220958; MSDS Number: 8962
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1200 SUS
1200 SUS
See Note 3.
Saybolt Viscosity at 210°F 93 SUS
93 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 18.1 cSt
18.1 cSt
See Note 3.
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 280
280
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
See Note 2.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
See Note 1.
Pour Point -12.0 °C
10.4 °F
See Note 3.
Flash Point 198 °C
388 °F
See Note 3.
Dropping Point 188 °C
370 °F
Descriptive Properties Value Comments
Color Brown
Corrosion, Copper Strip 1B
Texture Buttery
Thickener, % 7.5
Lithium