Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® NF-3017H PC/ABS, Unreinforced FR

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NF-3017H PC/ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 250 °C
16 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 70.6 MPa
10200 psi
50 mm/min; ASTM D638
Flexural Strength 108 MPa
15700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.70 GPa
391 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C

@Thickness 6.40 mm
201 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 1.00 - 3.00 mm
V-0

@Thickness 0.0394 - 0.118 in
Descriptive Properties Value Comments
Pencil Hardness F
500g, JIS K 5401
Users viewing this material also viewed the following: