Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrafil® J-1200/CF/40 NAT ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 40% Carbon Fiber Filled
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrafil® J-1200/CF/40 NAT ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 Hrs; ASTM D570
Linear Mold Shrinkage 0.00050 cm/cm
0.00050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 15.9 GPa
2300 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 18.0 - 21.6 µm/m-°C

@Temperature 20.0 °C
10.0 - 12.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.0 - 10 ohm
1.0 - 10 ohm
ASTM D648