Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 650 g | 1.43 lb | 26 in; ASTM D1709 |
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene
(discontinued **) Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce.. |
|||
Dart Drop Test | 650 g | 1.43 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Dart Drop Test | 650 g | 1.43 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Dart Drop Test | 650 g | 1.43 lb | ISO 7765-1 |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Dart Drop Test | 650 g | 1.43 lb | ASTM D1709A |
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing .. |
|||
Dart Drop Test | 650 g | 1.43 lb | F50; ISO 7765-A |
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. .. |
|||
Dart Drop Test | 650 g | 1.43 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Dart Drop Test | 650 g | 1.43 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |