Polymer Property : Elmendorf Tear Strength MD = 225 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 225 g
225 g
ASTM D1922
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin
Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals
Elmendorf Tear Strength MD 225 g
225 g
ASTM D1922
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene  (discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..
Elmendorf Tear Strength MD 225 g
225 g
ISO 6383-2
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and..
Elmendorf Tear Strength MD 225 g
225 g
ASTM D1922
Chevron Phillips MarFlex® D143 m-LLDPE Linear Low Density Polyethylene
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..
Elmendorf Tear Strength MD 225 g
225 g
ASTM D1922
Dow DOWLEX™ 2078G Linear Low Density Polyethylene
Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow