Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy duty packagingClarity packagingThis grade does contain a process aid.Information provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D1505
0.916 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm
5000 ppm
Slip Level 1000 ppm
1000 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 14.0 MPa
2030 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa
1450 psi
ASTM D882
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 600 %
600 %
ASTM D882
Puncture Energy 3.00 J
2.21 ft-lb
ASTM D3763
Coefficient of Friction 0.15
0.15
ASTM D1894
Elmendorf Tear Strength, MD 10.6 g/micron
270 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D1922
Dart Drop 23.6 g/micron
600 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 52.0 MPa
7540 psi
ASTM D882
Film Tensile Strength at Break, TD 51.0 MPa
7400 psi
ASTM D882
1% Secant Modulus, MD 174 MPa
25200 psi
ASTM D882
1% Secant Modulus, TD 190 MPa
27600 psi
ASTM D882
Heat Seal Strength Initiation Temperature 101 °C
214 °F
ASTM F882
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003
Gloss 95 %
95 %
at 60°; ASTM D2457
Descriptive Properties Value Comments
Film Puncture Force 46 N
ASTM D3763
Process Film
Region Mexico
Bamberger Polymers Distribution