Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 3.00 - 3.00 J @Temperature -30.0 - -30.0 °C |
2.21 - 2.21 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 2.65 J Grade Count:2 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Puncture Energy | 3.00 - 3.00 J @Load <=74.2 kg |
2.21 - 2.21 ft-lb @Load <=164 lb |
Average value: 2.65 J Grade Count:2 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Puncture Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Puncture Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Puncture Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers |
|||
Puncture Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers |
|||
Puncture Energy | 3.00 J @Load <=74.2 kg, Temperature -30.0 °C |
2.21 ft-lb @Load <=164 lb, Temperature -22.0 °F |
d.a.m.; ISO 6603-2 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Puncture Energy | 3.00 J | 2.21 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Puncture Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Puncture Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures |
|||
Puncture Energy | 3.00 J @Load <=74.2 kg, Temperature -30.0 °C |
2.21 ft-lb @Load <=164 lb, Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Puncture Energy | 3.00 J | 2.21 ft-lb | ASTM D3763 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |
|||
Puncture Energy | 3.00 J | 2.21 ft-lb | ASTM D3763 |
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Puncture Energy | 3.00 J | 2.21 ft-lb | DAM; ISO 6603-2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |