Polymer Property : Puncture Energy = 3.00 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 3.00 - 3.00 J

@Temperature -30.0 - -30.0 °C
2.21 - 2.21 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.65 J Grade Count:2
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Puncture Energy 3.00 - 3.00 J

@Load <=74.2 kg
2.21 - 2.21 ft-lb

@Load <=164 lb
Average value: 2.65 J Grade Count:2
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Puncture Energy 3.00 J

@Temperature -30.0 °C
2.21 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Puncture Energy 3.00 J

@Temperature -30.0 °C
2.21 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Puncture Energy 3.00 J

@Temperature -30.0 °C
2.21 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers
Puncture Energy 3.00 J

@Temperature -30.0 °C
2.21 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers
Puncture Energy 3.00 J

@Load <=74.2 kg,
Temperature -30.0 °C
2.21 ft-lb

@Load <=164 lb,
Temperature -22.0 °F
d.a.m.; ISO 6603-2
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Puncture Energy 3.00 J
2.21 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Puncture Energy 3.00 J

@Temperature -30.0 °C
2.21 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Puncture Energy 3.00 J

@Temperature -30.0 °C
2.21 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, good heat-ageing resistanceApplication Examples: pedal brackets, automotive front end structures
Puncture Energy 3.00 J

@Load <=74.2 kg,
Temperature -30.0 °C
2.21 ft-lb

@Load <=164 lb,
Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral
PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties
Puncture Energy 3.00 J
2.21 ft-lb
ASTM D3763
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer
Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films..
Puncture Energy 3.00 J
2.21 ft-lb
ASTM D3763
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Puncture Energy 3.00 J
2.21 ft-lb
DAM; ISO 6603-2
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per..